Here is a guide on how to make your own Ferric Chloride etchant. It’s a relatively simple process that only requires some iron, hydrochloric acid, and air. As the process uses acids please be careful, and do this only if you feel comfortable with it.

Get 20g of iron. This can be in the form of nails or steel wool. It’s best to use iron that’s rusting, that indicates it doesn’t have other metals like zinc or chromium that’s normally used to prevent rust. To the iron add 100mL of water and 100mL of 12M hydrochloric acid. The iron will start reacting with the acid to produce hydrogen gas and ferrous chloride. If the reaction is proceeding too slowly for your liking you can heat up the mixture. A flask of cold water on top is useful to reduce evaporative losses.

Side note: If you already have access to hydrochloric acid and hydrogen peroxide you might be better off just using that for etching. Here is an instructible on how to mix it up, and why it might be better then Ferric Chloride.

Via PCBheaven.

Join the Conversation

7 Comments

      1. Hmm, I guess you could act as suspicious as you like, as long as you don’t actually use it for meth, or have any iligal activities at home..

  1. Logical, lol. Some companies like the one I work for don’t ask and we’ve shipped stuff to people’s houses who were working on stained glass so you can tell them it is for electronic work.

Leave a comment

Leave a Reply to Rick Cancel reply

Your email address will not be published. Required fields are marked *

Notify me of followup comments via e-mail. You can also subscribe without commenting.